For many steel mills, the tundish lining itself can keep running for a long time. But the old fixed nozzle often gets worn or clogged first. This forces workers to stop casting and change the whole tundish. The exchange tundish nozzle solves this problem. It lets you swap the nozzle online and keep using the same tundish, so you run more heats in one sequence.

Why fixed nozzles limit casting sequence

Molten steel washes the nozzle bore nonstop during casting. Alumina buildup and slag corrosion make the nozzle hole bigger or blocked.

  • When the bore wears out, steel flow becomes unstable. Mold level jumps, casting speed is hard to hold.
  • If clogging gets worse, the steel stream twists or shrinks. You have to stop pouring and take the tundish offline.
  • Even if the tundish lining, stopper and insulation are still good, the whole tundish has to come out just because the nozzle fails. This cuts the sequence short and wastes refractory and steel.

How exchange nozzle works to extend sequence

The exchange nozzle assembly separates the replaceable metering part from the fixed upper nozzle and tundish brickwork. The tundish body stays in place on the caster.

  1. When the working nozzle is eroded or blocked, you slide in a preheated spare nozzle with the quick-change mechanism. No need to lift or remove the tundish.
  2. Good sealing stops air suction and steel leakage during hot swap. The steel stream keeps steady, and casting does not stop.
  3. You can do multiple nozzle swaps on one tundish. The tundish only comes out when its own lining reaches the end of service life.

Practical benefits on site

  • More heats per tundish. Many mills lift sequence heats greatly after switching to exchange nozzle. Less tundish change means fewer start-stop operations.
  • Less scrap and yield loss. Every tundish change brings extra crop and rejected billet. Fewer tundish changes cut this waste.
  • Lower refractory cost. You only replace the nozzle insert instead of the full tundish lining set.
  • Stable steel quality. Keep steady flow speed and good stream shape for longer time. Less air re-oxidation and inclusion trouble.
  • Flexible production. You can swap nozzles of different bore sizes online to adjust casting speed, match different steel grades and melting rhythm.

Key rules to get longer sequence

  1. Check nozzle condition regularly. Watch stream shape, mold level fluctuation and joint temperature. Do not wait until blockage or breakout risk appears.
  2. Always use preheated spare nozzles. Cold nozzle cracks right away after touching molten steel.
  3. Keep sealing faces clean. Damaged gasket or dirty contact surface causes air leak or steel seep, and you have to end sequence early.
  4. Control argon shield for clean steel grades. It slows alumina clogging and gives longer service for each working nozzle.
  5. Follow baking rules for new nozzle assembly. Thermal shock cracks will shorten nozzle life.

Common wrong operations that hurt sequence length

  • Delay nozzle change until the bore is heavily eroded.
  • Reuse old gaskets for hot exchange.
  • Skip preheating of standby nozzle.
  • Misalign the new nozzle after swap, causing biased steel scouring.
  • Overfill sealing mud and block the steel flow hole.

 

The exchange tundish nozzle does not make the tundish lining last forever. It removes the nozzle as the weak link that stops casting early. With proper inspection, hot exchange and sealing control, you fully use the service life of tundish lining. Steel plants run longer continuous sequences, reduce unplanned stops and bring down overall production cost.