Exchangeable Tundish Nozzle: Basic Knowledge for Steel Plants
Oct 22, 2026
Continuous casting operators know well that tundish nozzle is critical to control molten steel flow. Traditional fixed nozzle cannot be replaced online. Once blocked or worn, the tundish has to come offline directly. Changtai's exchangeable tundish nozzle solves this pain point. Below we sort out practical basics for site staff and purchasing team.
What It Is
It is a combined refractory assembly fitted at tundish bottom. The structure is split into fixed section and replaceable section. The upper nozzle and seat brick stay fixed on tundish. The lower metering nozzle can be hot changed while tundish remains on the caster. Workers use slide or swing quick-change mechanism to finish swap, and casting continues if sealing works properly. Changtai supplies full sets with zirconia metering core, matched for most billet and bloom casters.
Component List
- Upper nozzle: fixed inside seat brick, connects tundish inner cavity, bears molten steel static pressure
- Zirconia metering core (Changtai core part): controls steel flow rate, good anti-erosion and anti-clog performance
- Lower nozzle: guides steel stream, directly impacted by molten steel scouring
- Seat brick: supports the whole set and keeps concentricity
- Sealing gasket / refractory mud: seals contact surfaces, prevents steel leakage and air suction
- Quick-change base & clamping device: mechanical parts for hot exchange and locking
Working Logic
Install the whole Changtai nozzle set and complete baking before casting. During production, monitor steel stream and mould liquid level. When the running nozzle suffers erosion or clogging, slide the preheated spare nozzle into working position, lock the clamp and check sealing condition. The old nozzle moves away from flow channel. Tundish lining, stopper and heat preservation layer keep running.
On-site Advantages
✅ Longer casting sequence. No tundish shutdown just for nozzle failure, fully use lining service life
✅ Flexible flow adjustment. Swap different bore nozzles online to adjust casting speed for various steel grades
✅ Save refractory cost. Only replace worn lower nozzle instead of the whole tundish
✅ Reduce start-stop loss. Less tundish change means fewer crop and defective billets
✅ Stable steel quality. Good seal and smooth stream cut re-oxidation and inclusion defects
✅ Stable batch quality from Changtai. Strict density and size control, less bore enlargement.
Material Options from Changtai
- Zirconia core (90% / 93% / 96% ZrO₂): widely used for carbon steel and clean steel, good anti-clogging performance
- Alumina-carbon nozzle body: lower cost, suitable for common steel grades with low clog risk
- ZrO₂-CaO composite option: for steel grades easy to clog, self-clean effect for alumina deposit
Suitable & Unsuitable Scenarios
Fit: billet caster, bloom caster, long-sequence casting, low-carbon steel, Al-killed steel and clean steel production. Not the best fit: small batch, frequent grade switching, short tundish campaign.
Daily Check Items
- Inspect parts before installation. Scrap cracked, chipped or out-of-spec pieces. All Changtai products go through full inspection before delivery.
- Clean sealing surfaces thoroughly, remove slag and old residual mud
- Preheat standby nozzle before hot exchange. Cold nozzle cracks instantly touching molten steel
- Check stream shape after replacement. Skewed stream usually means offset or poor seal
- Watch joint temperature, smoke and steel seepage during casting
Simple Contrast
Fixed nozzle:No online change. Nozzle damage leads to tundish stop. Low initial cost, short sequence.
Changtai exchangeable nozzle:Hot swap available. Nozzle fault will not stop tundish. Higher upfront investment, longer sequence and lower total cost.