How to Prevent Air Aspiration on Tundish Slide Gate Plate?
Oct 16, 2026
Air aspiration is a common and tricky issue for tundish slide gate plates during continuous casting. Fast flowing molten steel creates negative pressure by venturi effect. Air gets sucked in through gaps, cracks or loose mating surfaces between slide plates. The incoming oxygen re-oxidizes molten steel, forms alumina inclusions, causes nozzle clogging and degrades final steel quality. In serious cases, it shortens plate service life and breaks casting sequence. Based on years of site experience, Changtai shares root causes and practical prevention methods.
Main Causes of Air Aspiration
- Poor sealing between plate contact faces. Uneven surface, scratches or residual slag leave tiny gaps. Under negative pressure, air is drawn into steel flow.
- Slide plate cracks. Thermal shock or wrong assembly creates microcracks, which become air leakage channels.
- Improper clamping force. Too loose bolts cannot keep plates tightly fitted; over-tight bolts lead to plate cracking during heating.
- Unstable argon protection. Wrong argon flow, gas line leaks or blocked gas channels fail to maintain positive pressure at plate joints.
- Operation fluctuations. Frequent gate opening/closing, unstable casting speed and low tundish bath depth worsen negative pressure inside the bore.
Practical Prevention Measures
- Control plate flatness and surface quality Select high-precision machined slide plates. Check surface scratches, pits and microcracks before assembly. Changtai slide gate plates are finished with strict flatness tolerance to keep full-area contact during sliding. Apply high temperature sealing coating on mating faces to fill micro gaps at working temperature.
- Standardize assembly and clamping Clean all contact surfaces thoroughly, remove slag and refractory debris. Set proper bolt torque, avoid over tightening or insufficient clamping. Ensure upper, middle and lower plates align correctly. Any misalignment will create local gaps when sliding.
- Optimize argon protection system Set suitable argon flow rate for the slide gate assembly. Argon builds slight positive pressure at plate joints to offset vacuum effect. Monitor argon back pressure in real time. Sudden pressure drop means gas leakage or air aspiration risk. Check gas pipeline and joints regularly to eliminate air mixing into argon. Do not use excessive argon, which triggers mold turbulence and steel defects.
- Stabilize casting parameters Keep stable tundish liquid level and steady casting speed. Avoid long-time small gate opening status, which easily generates strong negative pressure. Reduce frequent gate adjustment to lower pressure fluctuation at slide plate bore.
- Strict preheating and plate inspection Complete uniform preheating before casting to prevent thermal cracking. Reject plates with visible cracks or surface damage. Replace worn plates before gaps become larger.