What Causes Rapid Erosion of Tundish Slide Gate Plate Bore?
Oct 16, 2026
Tundish slide gate plate bore suffers fast wear and erosion in many continuous casting operations. Severe bore enlargement changes molten steel flow rate, disturbs casting stability and shortens plate service life. In extreme cases, uneven bore loss leads to steel breakout risk.
Key Reasons for Fast Bore Erosion
High speed molten steel scouring High casting speed and large steel flow create strong shear force on the inner bore wall. Molten steel continuously washes the refractory surface, stripping grain particles over time. Long duration of large gate opening accelerates this mechanical scouring.
Slag corrosion and penetration Tundish slag contains low melting point oxides. When slag contacts the bore, it dissolves the refractory bonding phase. The material surface softens and gets washed away easily. Low bath level allows more slag to enter the plate bore and worsen erosion.
Unsuitable refractory material grade Standard slide plate material cannot resist high scouring or special steel grades. For high carbon steel, alloy steel or high-speed casting, ordinary plates erode much faster. Poor sintering and low density also create loose structure, which steel and slag can attack easily.
Thermal cycling and surface spalling Repeated heating and cooling creates thermal stress on the bore surface. Tiny cracks form and peel off refractory grains. Once surface spalling starts, the fresh inner material is exposed directly to molten steel, speeding up bore enlargement.
Improper operation and gate movement Frequent opening and closing of slide gate causes friction wear on bore edge. Unstable steel flow, flow vortex and steel jet impact at bore inlet concentrate erosion at local positions.
Changtai's Recommended Solutions
Select proper plate grade Changtai high erosion resistant slide gate plates adopt high density sintered raw materials. Optimized grain structure improves resistance to steel scouring and slag corrosion. Match material grade with your steel type and casting speed.
Stabilize tundish liquid level and casting parameters Maintain stable tundish bath depth to reduce slag entering the bore. Avoid long time fully open gate. Keep steady casting speed to lower steel jet impact.
Control preheating quality Apply uniform preheating before casting to reduce thermal shock. Prevent surface microcracks and spalling on the bore inner wall.
Optimize argon protection Reasonable argon flow forms a protective layer along the bore wall. It lessens direct contact between molten steel and refractory, and reduces inclusion adhesion and local erosion.
Regular on-site inspection Check bore size during sequence change. Replace plates when bore diameter exceeds allowable limit to avoid abnormal casting accidents.
Rapid bore erosion of tundish slide gate plate is caused by combined mechanical scouring, slag chemical attack, material performance and casting operation. Proper refractory selection is fundamental. Stable tundish level, steady casting speed and standardized preheating effectively slow bore wear. Changtai provides customized slide gate refractories and technical support for continuous casting lines to extend plate service life.